Chapters0/30 ▾
Chapter 3 · Lesson 2 of 4
Wire rope slings: broken wires, wear and heat
1 min read
Broken wires are counted over one rope lay, the length in which one strand makes one full turn around the core. That window covers every strand once, so it is a fair place to count.
For a single-part, strand-laid sling, removal comes at ten randomly distributed broken wires in one lay or five broken wires in one strand within one lay. The second half of the rule is the one candidates drop: breaks bunched in one strand mean one load path is failing.
| Condition | ASME B30.9 | OSHA 1910.184 |
|---|---|---|
| Abrasion or scraping | More than 5 percent off the nominal rope diameter | One-third of the outside wire diameter |
| Fiber core heat limit | 180 degrees F | 200 degrees F |
Example: a 3/4 in rope measured under ASME is retired once severe local wear brings it below 0.75 x 0.95 = about 0.71 in. Kinking, crushing and birdcaging are removal conditions under both documents. So are heat damage, corrosion, and end attachments that are cracked, deformed or worn.
A kink is not straightened and put back to work, and a birdcaged section is not cut out in the field to save the rest; the sling is retired or sent to a qualified person for evaluation.
When the stem asks about a fiber core rope near a furnace, the answer is a sling rated for that heat, because a burned core loses its support for the strands while the outside can still look sound.
Check yourself
1. Under ASME B30.9, what number of broken wires in the body of a single-part, strand-laid wire rope sling requires removal from service?
2. When broken wires are counted "in one rope lay," what length of rope is that?
Facts checked 2026-11-15 · Sources: OSHA 29 CFR 1910.184: Slings, OSHA 29 CFR 1926.251: Rigging equipment for material handling, NCCCO: Rigger Level I written exam outline
Rigger Level I (NCCCO) cheat sheet: every key fact on one page →