Light-cured composite hardens only where enough light reaches it. Resin scatters and absorbs the beam, so it is placed in increments of about 2 mm, each cured before the next; dark and opaque shades need longer exposure.
A radiometer checks that the curing light still delivers enough intensity, because an aging light can look bright while its output has dropped. The tacky surface left on each cured layer is uncured monomer caused by oxygen in the air, and it is left alone because it bonds the next layer.
In total-etch bonding, 35 to 37 percent phosphoric acid removes the smear layer and opens the dentinal tubules. Etched dentin is then blotted, not blasted dry, because drying collapses the exposed collagen and the adhesive cannot soak in; etched enamel, in contrast, is dried to a frosty white.
Glass ionomer bonds chemically to tooth structure and releases fluoride over time, which makes it a good choice for root caries in a high-risk patient where isolation is hard.
Resin-modified glass ionomer adds a light-cured resin for more early strength and lower solubility. Example: a 3 mm deep composite box needs at least two increments, because 3 mm is more than one 2 mm layer.
Check yourself
1. After etched dentin is rinsed, why is it blotted rather than dried with a strong air blast?
2. A manufacturer directs that a composite be placed in increments of about 2 mm, each cured before the next. What does that increment limit address?